客服热线:18202992950

Stainless ball carbidecast iron material with 发明授权

2023-07-27 1770 1711K 0

专利信息

申请日期 2025-06-27 申请号 DE10230383
公开(公告)号 DE10230383B4 公开(公告)日 2009-11-26
公开国别 DE 申请人省市代码 全国
申请人 Osaka Prefecture Osaka JP; Kabushiki Kaisha Sankyogokin Juzosho Osaka JP; Nishiuchi Shigenori Hirakata Osaka JP; Kawano Yutaka Uji Kyoto JP; Yamamoto Satoru Kyoto Kyoto JP; OKAMOTO Co Ltd Gifu JP
简介 Spherical carbide cast iron material comprises iron as main component and contains 0.6-4.0 % carbon and 4-15 % vanadium as necessary components, 0.01-0.15 % phosphorus, 0.01-0.05 % sulfur, 0.05-1.0 % aluminum and 0.01-0.2 % magnesium as gas (hydrogen) bubble auxiliary aid, and 0.2-4.5 % silicon, 13-30 % chromium, 0.2-3.0 % manganese and 4-15 % nickel and/or cobalt as anticorrosion matrix former. Tiny spherical chambers of gas (hydrogen) bubbles are uniformly distributed into the molten metal whilst melting at 1673-1973 K and spherical vanadium carbide with a covalent bond is crystallized within the spherical chambers. Preferred Features : The spherical carbide cast iron material comprises iron as the main component and contains 0.6-4.0 % carbon (C) and 4-15 % vanadium (V) as necessary components, 0.01-0.15 % phosphorus (P), 0.01-0.05 % sulfur (S), 0.05-1.0 % aluminum (Al) and 0.01-0.2 % magnesium (Mg) as gas (hydrogen) bubble auxiliary aid, 0.1-1.5 % alloying elements of calcium (Ca), barium (Ba), strontium (Sr) and rare earth metals as gas (hydrogen) bubble stabilizer, and 0.2-4.5 % silicon (Si), 13-30 5 chromium (Cr), 0.2-3.0 % manganese (Mn) and 4-15 % nickel (Ni) and/or cobalt (Co) as anticorrosion matrix former.


您还没有登录,请登录后查看下载地址


反对 0举报 0 收藏 0 打赏 0评论 0
下载排行
网站首页  |  关于我们  |  联系方式  |  使用协议  |  版权隐私  |  网站地图  |  排名推广  |  广告服务  |  积分换礼  |  网站留言  |  RSS订阅  |  违规举报  |  京ICP备2021025988号-4