Magnetic alloy material and its manufacturing method 发明授权

2023-11-24 1810 940K 0

专利信息

申请日期 2025-06-28 申请号 JP2004323258
公开(公告)号 JP4371040B2 公开(公告)日 2009-11-25
公开国别 JP 申请人省市代码 全国
申请人 NEOMAX CO LTD
简介 PROBLEM TO BE SOLVED : To provide a method for manufacturing LaFe13-based alloy material with a higher efficiency than that of the prior art. SOLUTION : A rapid-cooled alloy manufacturing method includes the steps of : preparing molten raw alloy having a predetermined composition; and forming rapid-cooled alloy having a composition expressed by the compositional formula of Fe100-a-b-cREaAbTMc(wherein : RE is selected from a group consisting of La, Ce, Pr, Nd, Pm, Sm, Eu, Gd, Tb, Dy, Ho, Er and Tm and at least one kind of rare earth elements containing, by atom, ≥90 at.% La; A stands for Si and TM stands for Co; and 5 at.%≤a≤10 at.%, 4.7 at.%≤b≤18 at.%, and 0 at.%≤c≤9 at.%). COPYRIGHT : (C)2005, JPO&NCIPI


您还没有登录,请登录后查看下载地址


反对 0举报 0 收藏 0 打赏 0评论 0
下载排行
网站首页  |  关于我们  |  联系方式  |  使用协议  |  版权隐私  |  网站地图  |  排名推广  |  广告服务  |  积分换礼  |  网站留言  |  RSS订阅  |  违规举报  |  京ICP备2021025988号-4