申请人 COMMONWEALTH SCIENTIFIC AND INDUSTRIAL RESEARCH ORGANISATION
简介 An aluminium based alloy has a weight percentage composition of from 5 to 15% silicon, 0 to 0.25% magnesium, 0 to 0.25% titanium, 0.2 to 0.65% manganese, 0.1 to 0.6% iron, 1 to 4% copper, 0 to 3% zinc, less than 0.01% in total of silicon modifiers (with less than 0.007% strontium), less than 0.05% tin, less than 0.2% in total of other transition or rare earth metals (with less than 0.05% chromium), less than 0.5% in total other elements, and a balance of aluminium. The limits for iron and manganese are constrained such that the amount of iron present in the alloy is 0.4 to 1.6 times the manganese content and the alloy has a sludge factor (SF), calculated as SF=(1×wt % Fe)+(2×wt % Mn), of from 0.8 to 1.6. A casting made from the alloy has enhanced fracture resistance relative to casting of the same product made of a conventional HPDC alloy when compared in the as cast or same heat treated state.


您还没有登录,请登录后查看下载地址


反对 0举报 0 收藏 0 打赏 0评论 0
下载排行
网站首页  |  关于我们  |  联系方式  |  使用协议  |  版权隐私  |  网站地图  |  排名推广  |  广告服务  |  积分换礼  |  网站留言  |  RSS订阅  |  违规举报  |  京ICP备2021025988号-4