Magnesia spinel brick 发明授权

2023-09-02 4520 143K 0

专利信息

申请日期 2025-07-07 申请号 JP2002028133
公开(公告)号 JP4328053B2 公开(公告)日 2009-09-09
公开国别 JP 申请人省市代码 全国
申请人 KUROSAKI HARIMA CORP
简介 PROBLEM TO BE SOLVED : To improve the corrosion resistance of magnesia-spinel brick with rare earth oxide as refractories freed of chromium added when it is applied to the lining of a kiln for metal refining such as a steel secondary refining furnace. SOLUTION : In the magnesia-spinel brick with rare earth oxide added, Al2O3is not contained in a matrix, or the content thereof is prescribed to ≤2 mass%. The magnesia-spinel brick with rare earth oxide added has a raw material composition consisting of a magnesia clinker, a rare earth oxide raw material, and a spinel clinker, and, as for the grain size composition of the spinel clinker used as the raw material, the ratio of the ones with a grain size of ≥1 mm is 3 to 30 mass%, and the ratio of the ones with a grain size of COPYRIGHT : (C)2003, JPO


您还没有登录,请登录后查看下载地址


反对 0举报 0 收藏 0 打赏 0评论 0
下载排行
网站首页  |  关于我们  |  联系方式  |  使用协议  |  版权隐私  |  网站地图  |  排名推广  |  广告服务  |  积分换礼  |  网站留言  |  RSS订阅  |  违规举报  |  京ICP备2021025988号-4