Alloy, Protective Layer for Protecting a Component Against Corrosion and/or Oxidation at High Tempe 发明申请

2023-08-20 4360 590K 0

专利信息

申请日期 2025-07-15 申请号 US12085701
公开(公告)号 US20090155120A1 公开(公告)日 2009-06-18
公开国别 US 申请人省市代码 全国
申请人 STAMM WERNER
简介 Known protective layers with a high Cr content and additionally a silicon form brittle phases, which become even more brittle under the influence of carbon during use. The protective layer according to the invention has the composition 27% to 31% nickel, 23% to 29% chromium, 7% to 11% aluminum, 0.5% to 0.7% yttrium and/or at least one equivalent metal from the group comprising scandium and rare earth elements, optionally 0.6% to 0.8% silicon, optionally 0.5% to 0.7% zirconium and the remainder cobalt.