简介 PROBLEM TO BE SOLVED : To provide a poorly adhesive ceramic with a high corrosion resistance and a thermal shock resistance, which can be burned at a low temperature. SOLUTION : The poorly adhesive ceramic with a high corrosion resistance and a thermal shock resistance comprises an iron oxide ceramic containing unavoidable impurities as a parent phase and comprises 5-20 mass% high-melting metal oxide of the formula : MxOy (wherein M is at least one metal element chosen from Al, Mg, Ti, Zr and rare earth elements; and x and y satisfy the relations : 1≤x≤3 and 1≤y≤4; respectively) and 20-45 mass% Si3N4-Si2N2O-SiO2 compound particle dispersed in the parent phase. The high-melting metal oxide has a melting point of ≥1, 500°C, and the compound particle contains silicon (Si), oxygen (O) and nitrogen (N) elements. COPYRIGHT : (C)2008, JPO&INPIT


您还没有登录,请登录后查看下载地址


反对 0举报 0 收藏 0 打赏 0评论 0
下载排行
网站首页  |  关于我们  |  联系方式  |  使用协议  |  版权隐私  |  网站地图  |  排名推广  |  广告服务  |  积分换礼  |  网站留言  |  RSS订阅  |  违规举报  |  京ICP备2021025988号-4