Sintered rare earth magnet and its manufacturing method 发明授权

2023-06-02 2000 1141K 0

专利信息

申请日期 2025-07-08 申请号 JP2001224335
公开(公告)号 JP4081642B2 公开(公告)日 2008-04-30
公开国别 JP 申请人省市代码 全国
申请人 SHIN ETSU CHEM CO LTD
简介 PROBLEM TO BE SOLVED : To obtain an Sm2Co17-based sintered rare-earth magnet that will not cause hydrogen embrittlement, even if the magnet is used in a hydrogen atmosphere for a long time and can be used for a motor, etc., and to obtain a method of manufacturing the magnet. SOLUTION : The sintered rear-earth magnet is composed of 20-30 wt.% R (R : Sm or two or more kinds of rare-earth elements containing Sm at a rate of >=50 wt.%), 10-45 wt.% Fe, 1-10 wt.% Cu, 0.5-5 wt.% ZrO, and the balance Co and inevitable impurities. The magnet has a composite structure layer containing the Co and/or Sm2O3 and/or CoFe2O4 in the Co and Fe on its surface.


您还没有登录,请登录后查看下载地址


反对 0举报 0 收藏 0 打赏 0评论 0
下载排行
网站首页  |  关于我们  |  联系方式  |  使用协议  |  版权隐私  |  网站地图  |  排名推广  |  广告服务  |  积分换礼  |  网站留言  |  RSS订阅  |  违规举报  |  京ICP备2021025988号-4