RARE EARTH SINTERED MAGNET AND METHOD FOR PRODUCTION THEREOF 发明申请

2023-09-01 4440 1101K 0

专利信息

申请日期 2025-06-24 申请号 US11575928
公开(公告)号 US20090053094A1 公开(公告)日 2009-02-26
公开国别 US 申请人省市代码 全国
申请人 Hideyuki Morimoto; Tomoori Odaka
简介 A rare-earth sintered magnet includes 12.0 at % to 15.0 at % of rare-earth element(s), which is at least one element selected from the group consisting of Nd, Pr, Gd, Tb, Dy and Ho and at least 50% of which is Nd and/or Pr; 5.5 at % to 8.5 at % of boron (B); a predetermined percentage of additive metal A; and iron (Fe) and inevitably contained impurities as the balance. The predetermined percentage of additive metal A includes at least one of 0.005 at % to 0.30 at % of silver (Ag), 0.005 at % to 0.40 at % of nickel (Ni), and 0.005 at % to 0.20 at % of gold (Au).