HARDENED MARTENSITIC STEEL HAVING A LOW OR ZERO CONTENT OF COBALT, PROCESS FOR MANUFACTURING A PART 发明申请

2023-08-12 2870 1308K 0

专利信息

申请日期 2025-08-29 申请号 WOFR08051080
公开(公告)号 WO2009007562A1 公开(公告)日 2009-01-15
公开国别 WO 申请人省市代码 全国
申请人 AUBERT DUVAL SA; MONTAGNON JACQUES
简介 Steel characterized in that its composition is, in percentages by weight : - C = 0.20 - 0.30%; - Co = traces - 1%; - Cr = 2 - 5%; - Al = 1 - 2%; - Mo + W/2 = 1 - 4%; - V = traces - 0.3%; - Nb = traces - 0.1%; - B = traces - 30 ppm; - Ni = 11 - 16% with Ni ≥ 7 + 3.5 Al; - Si = traces - 1.0%; - Mn = traces - 2.0%; - Ca = traces - 20 ppm; - rare earths = traces - 100 ppm; - when N < 10 ppm, Ti + Zr/2 = traces - 100 ppm with Ti + Zr/2 < 10 N; - when 10 ppm < N < 20 ppm, Ti + Zr/2 = traces - 150 ppm; - O = traces - 50 ppm; - N = traces - 20 ppm; - S = traces - 20 ppm; - Cu = traces - 1%; - P = traces - 200 ppm, the remainder being iron and inevitable impurities resulting from the smelting. Process for manufacturing a part from this steel, and part thus obtained.


您还没有登录,请登录后查看下载地址


反对 0举报 0 收藏 0 打赏 0评论 0
下载排行
网站首页  |  关于我们  |  联系方式  |  使用协议  |  版权隐私  |  网站地图  |  排名推广  |  广告服务  |  积分换礼  |  网站留言  |  RSS订阅  |  违规举报  |  京ICP备2021025988号-4