Optical component and method for its production 发明申请

2023-02-26 3210 1237K 0

专利信息

申请日期 2025-06-25 申请号 US12222509
公开(公告)号 US20080315123A1 公开(公告)日 2008-12-25
公开国别 US 申请人省市代码 全国
申请人 Takayuki Komatsu; Tsuyoshi Honma; Takumi Fujiwara; Yasuhiko Benino
简介 To obtain an optical component having excellent secondary optical nonlinear properties by irradiating a surface and/or inside of glass having at least one member selected from Ni, Fe, V, Cu, Cr and Mn as a heat source material for absorbing and converting a laser beam to heat, incorporated to a glass matrix comprising at least one glass-forming oxide-selected from SiO2, GeO2, B2O3, P2O5, TeO2, Ga2O3, V2O5, MoO3 and WO3 and at least one member selected from alkali metals, alkaline earth metals, rare earth elements and transition elements, with a laser beam with a wavelength to be absorbed by the heat source material, to convert the irradiated portion to a single crystal or a group of crystal grains comprising components contained in the glass matrix and not containing the heat source material, thereby to form a pattern.


您还没有登录,请登录后查看下载地址


反对 0举报 0 收藏 0 打赏 0评论 0
下载排行
网站首页  |  关于我们  |  联系方式  |  使用协议  |  版权隐私  |  网站地图  |  排名推广  |  广告服务  |  积分换礼  |  网站留言  |  RSS订阅  |  违规举报  |  京ICP备2021025988号-4