MG ALLOY HAVING LOW C/A RATIO AND METHOD OF MANUFACTURING THE MG ALLOY SHEETS 发明授权

2023-08-26 1130 897K 0

专利信息

申请日期 2025-06-28 申请号 KR1020070033770
公开(公告)号 KR100860091B1 公开(公告)日 2008-09-18
公开国别 KR 申请人省市代码 全国
申请人 GALLOY TECHNOLOGY CO LTD
简介 An Mg alloy having a reduced axial ratio is provided to obtain excellent formability of the alloy at room temperature even without generating twins by activating electric potential movements in a basal slip system and a non-basal slip system during the plastic deformation and obtain excellent mechanical properties of the alloy by solution-strengthening the added elements in a matrix structure, and a method of manufacturing a Mg alloy sheet using the Mg alloy is provided. An Mg alloy having a reduced axial ratio is represented by the formula Mg100-x-yAxBy, wherein : the A is rare earth elements, one or more elements selected from commercialized alloys comprising the rare earth elements, or alloys thereof; the B is one or more elements selected from beryllium(Be), aluminum(Al), silicon(Si), cobalt(Co), nickel(Ni), copper(Cu), zinc(Zn), gallium(Ga), germanium(Ge), palladium(Pd), silver(Ag), cadmium(Cd), indium(In), tin(Sn), antimony(Sb), lead(Pb), bismuth(Bi), calcium(Ca), manganese(Mn), molybdenum(Mo), cobalt(Co), nitrogen(N), carbon(C), phosphorous(P), boron(B), and strontium(Sr); the x and y are 6 wt.% or less and 5 wt.% or less respectively; and the B has an axial ratio c/a of 1.61 or less that is defined as a ratio of a height(c) of the unit crystal to a side length(a) of a unit crystal of the Mg matrix by increasing solid solution of the A in the Mg matrix.


您还没有登录,请登录后查看下载地址


反对 0举报 0 收藏 0 打赏 0评论 0
下载排行
网站首页  |  关于我们  |  联系方式  |  使用协议  |  版权隐私  |  网站地图  |  排名推广  |  广告服务  |  积分换礼  |  网站留言  |  RSS订阅  |  违规举报  |  京ICP备2021025988号-4