简介 PROBLEM TO BE SOLVED : To provide a rare earth sintered magnet used for a motor, etc., that does not cause hydrogen brittleness even in a hydrogen atmosphere, by a method for manufacturing an R2Fe14B sintered magnet. SOLUTION : R (R is at least one kinds of rare earth elements selected out of Nd, Pr, Dy, Tb and Ho) of 20-35 wt.%, Co of 15 wt.% or less, B of 0.2-8 wt.%, at least one kinds of element, selected out of Ni, Nb, Al, Ti, Zr, Cr, V, Mn, Mo, Si, Sn, Ga, Cu and Zn, of 8 wt.% or less as an additive, and Fe and unavoidable impurities in residual part constitute an alloy. The alloy is fused and cast, and then crushed, finely pulverized, molded in a magnetic field, sintered and heat-treated in this order to make the sintered magnet. Further the sintered magnet is cut and/or ground to work a surface thereof, and then metal-plated. Then it is heat-treated at 80-700°C for 10 minutes to 50 hours. COPYRIGHT : (C)2003, JPO


您还没有登录,请登录后查看下载地址


反对 0举报 0 收藏 0 打赏 0评论 0
下载排行
网站首页  |  关于我们  |  联系方式  |  使用协议  |  版权隐私  |  网站地图  |  排名推广  |  广告服务  |  积分换礼  |  网站留言  |  RSS订阅  |  违规举报  |  京ICP备2021025988号-4