OPTICAL COMPONENT AND METHOD FOR MANUFACTURING THE SAME 发明申请

2023-03-22 1580 1875K 0

专利信息

申请日期 2025-07-08 申请号 WOJP07051731
公开(公告)号 WO2007091483A1 公开(公告)日 2007-08-16
公开国别 WO 申请人省市代码 全国
申请人 Nagaoka University of Technology; ASAHI GLASS CO LTD; KOMATSU Takayuki; HONMA Tsuyoshi; FUJIWARA Takumi; BENINO Yasuhiko
简介 Glass comprising at least one material, as a heat source material for absorbing and converting a laser beam to heat, selected from Ni, Fe, V, Cu, Cr, and Mn and added to a glass matrix comprising at least one glass forming oxide selected from SiO2, GeO2, B2O3, P2O5, TeO2, Ga2O3, V2O5, MoO3, and WO3 and at least one material selected from alkali metals, alkaline earth metals, rare earth elements, and transition elements is provided. A laser beam with a wavelength capable of absorbing the heat source material is applied to the surface and/or inside of the glass to convert the exposed part to a single crystal or a group of crystal grains free from the heat source material and comprising components contained in the glass matrix and thus to form a pattern. Thus, an optical component having excellent secondary optical nonlinear properties is obtained.


您还没有登录,请登录后查看下载地址


反对 0举报 0 收藏 0 打赏 0评论 0
下载排行
网站首页  |  关于我们  |  联系方式  |  使用协议  |  版权隐私  |  网站地图  |  排名推广  |  广告服务  |  积分换礼  |  网站留言  |  RSS订阅  |  违规举报  |  京ICP备2021025988号-4