Method of manufacturing sintered magnet 发明授权

2023-06-25 4830 110K 0

专利信息

申请日期 2025-06-27 申请号 JP11375642
公开(公告)号 JP3960730B2 公开(公告)日 2007-08-15
公开国别 JP 申请人省市代码 全国
申请人 TDK Corporation3067
简介 PROBLEM TO BE SOLVED : To improve remanent magnetic flux density by improving the density of a sintered body in a sintered ferrite magnet, which is manufactured by using a dry molding method which is low cost to carryout but hard to obtain good characteristics. SOLUTION : This sintered magnet comprises, as main components, A, R, Fe and M, where A is selected from among Sr, Ba and Pb while positively including Sr, R is selected from Y, rare earth elements and Bi while positively including La, and M includes Co or, Co and Zn. When the main component A is represented by formula A1-xRx(Fe12-yMy)zO19, it results in that 0.04<=x<=0.45, 0.40<=y<=0.3, 0.9<=x/y<=1.5, 0.95<=z<=1.05. Furthermore, the magnet comprises, as subcomponents, SiO2 and CaO, and the ratio of the subcomponents with respect to the main components is 0.42 to 0.84 wt.%, while the molar ratio of Ca/Si is in the range of 1.3 to 2.2.


您还没有登录,请登录后查看下载地址


反对 0举报 0 收藏 0 打赏 0评论 0
下载排行
网站首页  |  关于我们  |  联系方式  |  使用协议  |  版权隐私  |  网站地图  |  排名推广  |  广告服务  |  积分换礼  |  网站留言  |  RSS订阅  |  违规举报  |  京ICP备2021025988号-4