METHOD OF PREVENTING HYDROGEN EMBRITTLEMENT OF SINTERED RARE EARTH MAGNET 发明申请

2023-11-29 2970 529K 0

专利信息

申请日期 2025-06-25 申请号 JP2006285962
公开(公告)号 JP2007116171A 公开(公告)日 2007-05-10
公开国别 JP 申请人省市代码 全国
申请人 SHINETSU CHEMICAL CO
简介 PROBLEM TO BE SOLVED : To provide a Sm2Co17-based sintered magnet capable of solving a problem that hydrogen embrittlement occurs in a hydrogen atmosphere and thereby chipping, cracking, or powdering occur. SOLUTION : There is provided a method of preventing hydrogen embrittlement of a sintered rare earth magnet, wherein in a sintered rare earth magnet composed of R (wherein R is Sm or two or more kinds of rare-earth elements containing Sm of 50 wt.% or more) of 20-30 wt.%, Fe of 10 to 45 wt.%, Cu of 1 to 10 wt.%, Zr of 0.5 to 5 wt.%, a balance Co, with inevitable impurities, on the surface of this magnet, a metal oxide layer and/or a metal nitride layer is formed directly or through plated metallic layers. By a Sm2Co17-based sintered magnet of the present invention, it is possible to obtain a sintered rare earth magnet that does not cause hydrogen embrittlement even in a hydrogen atmosphere and can be used for motors, etc. COPYRIGHT : (C)2007, JPO&INPIT


您还没有登录,请登录后查看下载地址


反对 0举报 0 收藏 0 打赏 0评论 0
下载排行
网站首页  |  关于我们  |  联系方式  |  使用协议  |  版权隐私  |  网站地图  |  排名推广  |  广告服务  |  积分换礼  |  网站留言  |  RSS订阅  |  违规举报  |  京ICP备2021025988号-4