METHOD OF MANUFACTURING DIELECTRIC CERAMIC COMPOSITION 发明申请

2023-06-27 4940 187K 0

专利信息

申请日期 2025-07-09 申请号 JP2005252411
公开(公告)号 JP2007063077A 公开(公告)日 2007-03-15
公开国别 JP 申请人省市代码 全国
申请人 TDK CORP
简介 PROBLEM TO BE SOLVED : To provide a dielectric ceramic composition having a specific dielectric constant εr of ≥200, a temperature characteristic τε of the dielectric constant of ≤200 ppm/K, and an excellent Q characteristic. SOLUTION : In manufacturing a dielectric ceramic composition having a basic compositional component represented by aMO-bLiO1/2-cBiO3/2-dREO3/2-eTiO2[wherein M is at least one kind selected from Ba, Sr, Ca and Mg; RE is at least one kind selected from rare-earth elements; a+b+c+d+e=100(mol%); 10≤a≤25; 10≤b≤20; 8≤c≤15; 2≤d≤10; 50≤e≤60; and 0.65≤b/(c+d)≤1.0], the ceramic composition is sintered in an oxygen atmosphere having a higher oxygen concentration than that of the ambient air. Alternatively, the sintered compact can be annealed in an oxygen atmosphere having a higher oxygen concentration than that of the ambient air. The oxygen concentration of the atmosphere of high oxygen concentration is preferably 25% or more. COPYRIGHT : (C)2007, JPO&INPIT


您还没有登录,请登录后查看下载地址


反对 0举报 0 收藏 0 打赏 0评论 0
下载排行
网站首页  |  关于我们  |  联系方式  |  使用协议  |  版权隐私  |  网站地图  |  排名推广  |  广告服务  |  积分换礼  |  网站留言  |  RSS订阅  |  违规举报  |  京ICP备2021025988号-4