ALUMINUM FOIL FOR ELECTROLYTIC CAPACITOR ELECTRODE, AND MANUFACTURING METHOD THEREFOR 发明申请

2023-04-25 1010 156K 0

专利信息

申请日期 2025-06-28 申请号 JP2005230492
公开(公告)号 JP2007046093A 公开(公告)日 2007-02-22
公开国别 JP 申请人省市代码 全国
申请人 MITSUBISHI ALUMINIUM
简介 PROBLEM TO BE SOLVED : To provide aluminum foil for electrolytic capacitor electrode in which foil thickness can be increased and higher capacitance can be attained and also to provide its manufacturing method. SOLUTION : When manufacturing the aluminum foil for electrolytic capacitor electrode which has a purity of ≥99.9% and a composition consisting of 5 to 30 ppm Si, 5 to 30 ppm Fe, 10 to 100 ppm Cu, 0.1 to 3 ppm Pb and the balance Al with inevitable impurities and further containing, if necessary, 1 to 20 ppm, in total, of one or more elements among Li, Na, Ca and rare earth elements, and also has 111 to 200μm foil thickness, degassing treatment is performed at casting to regulate a gas value in a casting to ≤0.12 cc/100g and final annealing is carried out at ≥550°C for 6 h. By this method, the aluminum foil for electrolytic capacitor electrode in which cubic crystal rate is made to ≥95% and the area ratio of coarse crystal grains of ≥5 mm circle-equivalent diameter is made to ≤0.01% can be obtained and high capacitance can be attained. COPYRIGHT : (C)2007, JPO&INPIT


您还没有登录,请登录后查看下载地址


反对 0举报 0 收藏 0 打赏 0评论 0
下载排行
网站首页  |  关于我们  |  联系方式  |  使用协议  |  版权隐私  |  网站地图  |  排名推广  |  广告服务  |  积分换礼  |  网站留言  |  RSS订阅  |  违规举报  |  京ICP备2021025988号-4