REAR EARTH SINTERED MAGNET AND MANUFACTURING METHOD THEREOF 发明申请

2023-11-02 3400 65K 0

专利信息

申请日期 2025-06-27 申请号 JP2005233110
公开(公告)号 JP2007049010A 公开(公告)日 2007-02-22
公开国别 JP 申请人省市代码 全国
申请人 NEOMAX CO LTD
简介 PROBLEM TO BE SOLVED : To provide a rear earth sintered magnet wherein its residual magnetic-flux density is improved in comparison with the case of Al and Cu being added to it, while exhibiting its coercive force nearly equal to its coercive force obtained in the case of Al and Cu being added to it. SOLUTION : The rear earth sintered magnet contains rear earth elements R of 12.0-15.0 atom% (R are one or more elements selected from the group comprising Nd, Pr, Gd, Tb, Dy, and Ho, and contain Nd/Pr not less than 50%), B of 5.5-8.5 atom%, Ni of 0.005-0.40 atom%, Fe of the residual portion, and unavoidable impurities. COPYRIGHT : (C)2007, JPO&INPIT


您还没有登录,请登录后查看下载地址


反对 0举报 0 收藏 0 打赏 0评论 0
下载排行
网站首页  |  关于我们  |  联系方式  |  使用协议  |  版权隐私  |  网站地图  |  排名推广  |  广告服务  |  积分换礼  |  网站留言  |  RSS订阅  |  违规举报  |  京ICP备2021025988号-4