申请日期 | 2025-06-26 | 申请号 | JP10084599 |
公开(公告)号 | JP3856939B2 | 公开(公告)日 | 2006-12-13 |
公开国别 | JP | 申请人省市代码 | 全国 |
申请人 | Kyocera Corporation6633 | ||
简介 | PROBLEM TO BE SOLVED : To provide both an engine part having a low thermal conductivity and a high strength at high temperatures and a method for producing the engine part. SOLUTION : This engine part is formed from ceramics obtained by sintering a molded product prepared by compounding 80-95.5 wt.% of a cordierite powder having =80 MPa strength at 800 deg.C. |