SELECTIVELY LIGHT PENETRATE COMPOSITION, METHOD OF MANUFACTURING THE SELECTIVELY LIGHT PENETRATE LA 发明申请

2023-09-11 2960 230K 0

专利信息

申请日期 2026-03-15 申请号 KR1020050045382
公开(公告)号 KR1020060123807A 公开(公告)日 2006-12-05
公开国别 KR 申请人省市代码 全国
申请人 SAMSUNG CORNING CO LTD
简介 PURPOSE : A selectively light-transmissive matter, a selectively light-transmissive layer producing method having the same, and a light source device are provided to selectively transmit the light generated from the inside by making a selectively light-transmissive layer of the selectively light-transmissive matter containing rare-earth metallic oxide and disposing the selectively light-transmissive layer on the front side of an upper substrate.CONSTITUTION : The selectively light-transmissive matter for forming a selectively light-transmissive layer(150) consists of glass powder with a low melting point of 80-99wt.%% and rare-earth metallic oxides of 1-20wt.%%. A softening point of the glass powder having a low melting point is within a range of 350-550 deg.C. The rare-earth metallic oxide is Nd203(Neodymium) and Pr5011(Praseodymium) or the mixture thereof. The light-transmissive matter contains the rare-earth metallic oxides of 0.9-17wt.%% and a colorant of 0.1-3wt.%%.? KIPO 2007


您还没有登录,请登录后查看下载地址


反对 0举报 0 收藏 0 打赏 0评论 0
下载排行
网站首页  |  关于我们  |  联系方式  |  使用协议  |  版权隐私  |  网站地图  |  排名推广  |  广告服务  |  积分换礼  |  网站留言  |  RSS订阅  |  违规举报  |  京ICP备2021025988号-4