The rare-earth permanent magnet 发明授权

2023-09-13 1190 69K 0

专利信息

申请日期 2025-08-28 申请号 JP07213120
公开(公告)号 JP3777205B2 公开(公告)日 2006-05-24
公开国别 JP 申请人省市代码 全国
申请人 Isuzu Motors Ltd170
简介 PROBLEM TO BE SOLVED : To attain high magnetic characteristics by filling a die with an anisotropic powder produced by pulverizing a rare earth based alloy powder through hydrogen occlusion and emission and then subjecting the anisotropic powder to conduction sintering in specified heating pattern thereby solidifying the anisotropic powder. SOLUTION : A material rare earth based alloy powder is pulverized by oxygen occlusion and emission to produce an anisotropic powder which then fills a die for producing a final product shape and subjected to pressure molding. The die is set in a conduction sintering system for heating the powder by conducting a current directly through the powder. A heating pattern for temporarily inducing phase separation reaction of oxygen in the solidification of anisotropic powder containing (residual) hydrogen and then causing recombination reaction in the solidification process is realized through a quick heating and cooling. Quick heating and cooling is carried out at 600-900 deg.C for 0.5-10min.


您还没有登录,请登录后查看下载地址


反对 0举报 0 收藏 0 打赏 0评论 0
下载排行
网站首页  |  关于我们  |  联系方式  |  使用协议  |  版权隐私  |  网站地图  |  排名推广  |  广告服务  |  积分换礼  |  网站留言  |  RSS订阅  |  违规举报  |  京ICP备2021025988号-4