客服热线:18202992950

METHOD OF MANUFACTURING RARE EARTH SINTERED MAGNET AND METHOD OF PULVERIZING RAW ALLOY POWDER FOR SI 发明申请

2023-01-31 4100 194K 0

专利信息

申请日期 2025-06-24 申请号 JP2005184751
公开(公告)号 JP2006041501A 公开(公告)日 2006-02-09
公开国别 JP 申请人省市代码 全国
申请人 TDK CORP
简介 PROBLEM TO BE SOLVED : To provide a manufacturing method of a rare earth sintered magnet suppressing the amount of a lubricant added to the utmost and obtaining a compact with high strength and a sintered magnet with high magnetic characteristics, and a method of pulverizing raw alloy powder for the sintered magnet. SOLUTION : In manufacturing a rare earth sintered magnet, a lubricant having a particle size of 425 μm or below is added to the coarsely pulverized powder obtained by coarsely pulverizing a raw alloy. Then, it is pulverized by a jet mill to obtain finely pulverized powder. Then, this finely pulverized powder is formed in a magnetic field to form a compact. This compact is sintered to obtain the rare earth sintered magnet. To bring the particle size to 425 μm or below in the lubricant, the lubricant is preferably pulverized in a frozen state and classified. COPYRIGHT : (C)2006, JPO&NCIPI


您还没有登录,请登录后查看下载地址


反对 0举报 0 收藏 0 打赏 0评论 0
下载排行
网站首页  |  关于我们  |  联系方式  |  使用协议  |  版权隐私  |  网站地图  |  排名推广  |  广告服务  |  积分换礼  |  网站留言  |  RSS订阅  |  违规举报  |  京ICP备2021025988号-4