分享好友 知识库首页 频道列表

Improvement of flowability of resin

2025-07-27 19:093650下载
文件类型:PDF文档
文件大小:213K
PROBLEM TO BE SOLVED : To provide a method capable of improving melt fluidity of a thermoplastic resin.SOLUTION : A structural unit represented by formula (1a) and/or (1b) is introduced into a thermoplastic resin to improve melt fluidity of the thermoplastic resin. (In the formula, Rand Rare the same or different and each represent an optionally substituted alkylene group; Rrepresents an inert substituent; m represents an integer of 0-4; and k represents 0 or an integer of 1-4.)