文件类型:PDF文档
文件大小:1077K
[Problem]We provide a method for producing nitride phosphors that can exhibit high luminescence intensity. [Solution means] A compound containing at least one rare earth element selected from the group consisting of Y, La, Ce, Lu and Gd is heat treated at a temperature within a range of 800 ° C. or more and 1800 ° C. or less to obtain a first heat treatment product having a crystaltron diameter of 150 nm or more, and the first heat treatment material and, if necessary, Y, as a raw material including the first heat treatment material and as necessary. It is a method for producing a nitride phosphor comprising a M source comprising at least one rare earth element M selected from the group consisting of Lu and Gd, a Mixture prepared so that the raw material includes a La source, a Si source, a Ce source, and a preparation composition indicated by the composition formula LawMxSi6Ny : Cez is heat treated at a temperature within a range of 1200 ° C. or more and 1800 ° C. or less. However, in the composition formula, w, x, y and z are 0. 5≦w≦4. 5、0<x≦1. 5、0≦y≦12、0<z≦1. 5、0. 15<(x+z)<3. 0、3. 0≦(w+x+z)≦7. Meet 5. [Selection Figure]Figure 3