The present invention relates to an RFeB sintered magnet containing : 28% to 33% by mass of a rare-earth element R, 0% to 2.5% by mass of Co (cobalt) (i.e., Co may not be contained), 0.3% to 0.7% by mass of Al (aluminum), 0.9% to 1.2% by mass of B (Boron), and less than 1, 500 ppm of O (oxygen), with the balance being Fe, containing an RFeAl phase having an R6Fe14-xAlx structure in a crystal grain boundary, and having a coercivity of 16 kOe or more.