文件类型:PDF文档
文件大小:603K
To provide a method of producing a spherical aluminum nitride powder which has a large thermal conductivity and excellent filling property, and is useful as a filler for heat-radiating materials.
[Means for Solution]
The spherical aluminum nitride powder is produced by reductively nitriding a mixture of 100 parts by mass of an alumina or an alumina hydrate, 0.5 to 30 parts by mass of a rare earth metal compound and 38 to 46 parts by mass of a carbon powder at a temperature of 1620 to 1900°C for not less than 2 hours.