A method of making LSO scintillators with high light yield and short decay times is disclosed. In one arrangement, the method includes codoping LSO with cerium and another dopant from the IIA or IIB group of the periodic table of elements. The doping levels are chosen to tune the decay time of scintillation pulse within a broader range (between about ˜30 ns up to about ˜50 ns) than reported in the literature, with improved light yield and uniformity. In another arrangement, relative concentrations of dopants are chosen to achieve the desired light yield and decay time while ensuring crystal growth stability.