文件大小:1153K
There is provided a method for preparing a β-SiAlON phosphor capable of be controlled to show characteristics such as high brightness and desired particle size distribution. The method for preparing a β-SiAlON phosphor represented by Formula : Si(6-x)AlxOyN(8-y) : Lnz (wherein, Ln is a rare earth element, and the following requirements are satisfied : 0
点赞 0
反对 0
举报 0
收藏 0
打赏 0
评论 0

- 一种用于声磁标签材料的非晶带
0下载498浏览232K

- 一种利用生物质制备苯甲酸的方法
0下载280浏览407K

- 一种连续式网带炉用奥氏体耐热合金网带丝配方及其制备方法
0下载432浏览655K

- CE- and zirconium-base mixed oxides
0下载321浏览4806K

- 有机阴离子柱撑稀土氢氧化物纳米片溶胶的制备方法
0下载111浏览786K

- 一种连续制备双面织构高温超导二代带材过渡层的方法
0下载214浏览1222K

- 一种催化裂化催化剂及其制备方法
0下载138浏览920K