A permanent magnet comprises boron, cobalt, a metallic alloy component, about 28-35 weight percent of mixed rare-earth material, and iron as a balance. The metallic alloy component is selected from the group consisting of aluminum, copper, niobium, gallium, vanadium, chromium, zirconium, and combinations thereof. The mixed rare-earth material comprises light rare-earth material and heavy rare-earth material. The light rare-earth material comprises at least about 50 weight percent of praseodymium and about 5-50 weight percent of neodymium. The heavy rare-earth material comprises dysprosium or a combination of dysprosium and terbium. The mixed rare-earth material comprises about 3-45 weight percent of heavy rare-earth material. A sum of intrinsic coercivity in the unit of kilo Oersted (kOe) and maximum energy product in unit of mega gauss Oersteds (MGOe) of the permanent magnet is at least about 55.


请登录查看


反对 0
举报 0
收藏 0
打赏 0
评论 0