文件类型:PDF文档
文件大小:120K
PROBLEM TO BE SOLVED : To provide a method which can produce a rare earth alloy powder having superior magnetic properties by using a HDDR method.
SOLUTION : The method for producing the rare earth alloy powder by using the HDDR method includes : a hydrogenolysis step (II) of subjecting a raw material alloy which contains ρ (mass%) of a rare earth element to hydrogenolysis at the temperature of T1 to obtain a decomposed product having the hydrogen concentration of η1 (mass%); a first desorption recombination step (IV) of releasing hydrogen from the decomposed product at a predetermined velocity at the temperature of T2 which is higher than the temperature of T1 to lower the hydrogen concentration in the decomposed product from η1 to η2 (mass%) which satisfies following expression (1) : 0.008×ρ≤η2≤0.013×ρ (1); and a second desorption recombination step (V) of lowering the rate of releasing hydrogen from the decomposed product compared to that in the first desorption recombination step (IV) to further lower the hydrogen concentration in the decomposed product and obtain the rare earth alloy powder.
COPYRIGHT : (C)2011, JPO&INPIT