文件类型:PDF文档
文件大小:121K
PROBLEM TO BE SOLVED : To provide a method for producing clathrate compounds from the melt of the constituents thereof.
SOLUTION : The present invention relates a method for producing clathrate compounds, comprising producing a homogeneous melt containing the desired elements in the desired ratio, and subsequently solidifying the melt to obtain the clathrate compound by quickly cooling the same. A preferable matrix or cage component(s) is one or more elements selected from Si, Ge, Sn, Pb, Al, Ga, In and transition elements, and a preferable clathrating component(s) is one or more elements selected from alkali metals, alkaline-earth metals and transition metals including lanthanoids and actinoids, and, more preferably, one or more elements selected from alkaline-earth elements, lanthanoids, and ocationally, actinoids. These elements are preferable for the production of clathrate for thermoelectric and semiconductor applications.
COPYRIGHT : (C)2010, JPO&INPIT