Silver oxide superconductor containing and its manufacturing method

2025-06-19 21:502850下载
文件类型:PDF文档
文件大小:407K
PROBLEM TO BE SOLVED : To improve electromagnetic characteristics in air by adding a silver- contg. compd. to a source mixture of specified compds., melting the mixture in air at a temp. higher than the temp. to cause partial melting, keeping the mixture at a specified temp. or slowly cooling. SOLUTION : A source material mixture containing a RE compd. (RE is a rare earth metal element including Y), a Ba compd. and a Cu compd. is mixed with Al metal or an Al compd. by 1 to 60 wt.% (calculated as the weight of only Al element) and molten at a temp. higher than the temp. to cause partial melting in an atmosphere of 2×10 to 1 atm oxygen partial pressure P0 . Then the mixture is cooled to room temp. or if necessary kept at a specified temp. and slowly cooled to obtain an oxide superconductor having a phase of RE2(1-q) Ba1+r CuO5+s or a phase of RE4(1-q) Ba2(1+r) Cu2 O2(5+s) in a phase of RE1+x Ba2+y Cu3 Od phase. In the formulae, x, y, d satisfy -0.3
反对 0
举报 0
收藏 0
打赏 0
评论 0