PROBLEM TO BE SOLVED : To provide a method of manufacturing a natural radioactive rare element mineral protruded product whose content rate is at least 50% to utilize the effect of the natural radioactive rare element mineral to the maximum.
SOLUTION : A several-micron natural radioactive rare element granular material is blended with an adhesive (such as an acrylic, water-soluble, or solvent adhesive) and applied in a screen printing manner to a base material (regardless of the material such as a fabric, plastic, wood or metal), so that the natural radioactive rare element mineral protruded product with at least 50% content rate can be manufactured. Further, fitness gear which can make the most of the characteristics of the natural radioactive rare element mineral can be manufactured.
COPYRIGHT : (C)2006, JPO&NCIPI