Austenitic alloy for heat strength with improved pouring and manufacturing, process for manufacturi

2025-07-27 04:191630下载
文件类型:PDF文档
文件大小:851K
Austenitic alloy for high-temperature strength with improved pourability and manufacturing, of which the composition comprises, in weight-% : 0.010%−41 where eq. Crb=Cr+0.7×Si+1.37×Mo+3×Ti+6×Al+4×V, and where eq. Nib=Ni+22×C+0.5×Cu+0.5×Mn.[/in-line-formulae]