A production method for a rare earth permanent magnet, wherein : a sintered magnet body comprising an R1—Fe—B composition (R1 represents one or more elements selected from among rare earth elements, including Y and Sc) is immersed in an electrodeposition liquid obtained by dispersing a powder containing an R2 oxyfluoride and/or an R3 hydride (R2 and R3 represent one or more elements selected from among rare earth elements, including Y and Sc) in a solvent; an electrodeposition process is used to coat the powder onto the surface of the sintered magnet body; and, in the state in which the powder is present on the surface of the magnet body, the magnet body and the powder are subjected to a heat treatment in a vacuum or an inert gas at a temperature equal to or less than the sintering temperature of the magnet.