The present invention provides a method and apparatus for preparing a rare earth-activated barium fluorohalide based phosphor, in which atmospheric states during calcining and during cooling can be optimally adjusted and a cooling rate can be selected in a wide range. In the preparing apparatus of the present invention, a mixture 18 of phosphor materials is calcined by a calcining furnace 10 to form a calcined product, and thereafter, the calcined product is cooled to thereby prepare a rare earth-activated barium fluorohalide based phosphor. A calcining region 12 in which the mixture of phosphor materials can be calcined is provided in the calcining furnace 10, and a portion of the calcining region 12 is connected, via a partition door 30 capable of being opened and closed, to a cooling region 28 in which the calcined product can be cooled, at an outer side of the calcining furnace 10. Further, the method for preparing the rare earth-activated barium fluorohalide based phosphor of the present invention is carried out by using the above-described preparing apparatus.