Silicon nitride anti-wear member (2) characterized in that it is constituted of a ceramic sintered compact comprising 55 to 75 mass%% of silicon nitride, 12 to 28 mass%% of silicon carbide, 3 to 15 mass%%, in terms of silicide, of at least one element selected from the group consisting of Mo, W, Ta and Nb and 5 to 15 mass%% of grain boundary phase constituted of rare earth element-Si-Al-O-N and that the silicon nitride anti-wear member exhibits an electric resistance of 107 to 104 Ω · cm, a porosity of 1%% or less and a 3-point bending strength of 900 MPa or more. These enable providing a silicon nitride anti-wear member which exhibits not only intrinsic high strength and high toughness of silicon nitride but also given electrical resistance (conductivity) and which is especially excellent in sliding characteristics; and further providing a process for producing such a silicon nitride anti-wear member. © KIPO & WIPO 2007


请登录查看


反对 0
举报 0
收藏 0
打赏 0
评论 0