PHOTOSTIMULABLE PHOSPHOR, MANUFACTURING METHOD THEREFOR, AND RADIOLOGICAL IMAGE CONVERSION PANEL

2025-06-17 16:594470下载
文件类型:PDF文档
文件大小:71K
PROBLEM TO BE SOLVED : To provide a photostimulable phosphor which is excellent in photostimulation luminescence intensity, shows little X-ray damage, and has a good granularity; a manufacturing method for the phosphor; and a radiological image conversion panel. SOLUTION : In the manufacturing method for the photostimulable phosphor of the formula (1) : (Ba1-xM1)FBryI1-yX : aM2, bLn, cO (wherein M1 is at least one alkaline earth metal atom selected from the group consisting of Mg, Ca, Sr, Zn, and Cd; M2 is at least one alkali metal atom selected from Li, Na, K, Rb, and Cs; X is at least one halogen atom selected from Cl, Br, and I; Ln is at least one rare-earth atom selected from Ce, Pr, Sm. Eu, Gd, Tb, Tm, Dy, Ho, Nd, Er, and Yb; and (x), (y), (a), (b), and (c) satisfy the relations : 0≤x≤0.3, 0≤y≤0.3, 0≤a≤0.05, 0